Inicio / Productos / Soldadura inoxidable / Alloy Wire / Resistive alloy wires

Stainless Steel Welding / Alloy Wire / Resistive alloy wires

INALLOY 80

Nominal Composition:
• Ni 76,0 min
• Cr 19,0-21,0
• Si  0,5-2.0
• Mo 0,6

Material Characteristics:

- Specific resist. at 20 °C 108 micro ohm/cm
- Density 8,40 g/cm3
- Temp. coefficient of resistance 60 km x 10-6 / °C
- T. range 20 - 1000 °C
- Approx. Melting Point 1400 °C

Applications:

Open and metal sheathed elements for domestic and industrial appliances. Control resistors. Coil resistors and potentiometers. Widely used for the electric and electronic industries.

Reference norms:
- ASTM B344 80NI-20CR
- DIN 17470 NiCr 80 20 - Wst 2.4869

INALLOY 60

Nominal Composition:
• Ni 59,0-65,0 min
• Fe 19,0-25,0
• Cr 14,0-18,0
• Si 0,75-1,60 • Mn 1,0 max
• Cu 0,5 max
• C 0,15 max6

Material Characteristics:

- Specific resist. at 20 °C 112 micro ohm/cm
- Density 8,25 g/cm3
- Temp. coefficient of resistance 170 km x 10-6 / °C
- T. range 20 - 500 °C
- Approx. Melting Point 1350 °C

Reference norms:
- ASTM B344 60NI-16CR
- DIN 17470 NiCr 60 15 - Wst 2.4867

INALLOY 40

Nominal Composition:
• Ni 35,0-38,0 min
• Cr 19,0-21,0
• Si 1,0-3,0
• Mn 1,0 max
• Cu 0,5 max
• C 0,15 max
• Fe rim.

Material Characteristics:

- Specific resist. at 20 °C 105 micro ohm/cm
- Density 7,95 g/cm3
- Temp. coefficient of resistance 240 km x 10-6 / °C
- T. range 20 - 1000 °C
- Approx. Melting Point 1380 °C

Reference norms:
- ASTM B344 35NI-20CR

ICRALLOY 25

Nominal Composition:
• Cr 22,0-25,0
• Al 4,5-6,0
• Si 1,0 max
• Mn 0,6 max
• C 0,10 max
• Fe rem.

Material Characteristics:

- Specific resist. at 20 °C 144 micro ohm/cm
- Density 7,10 g/cm3
- Temp. coefficient of resistance 35 km x 10-6 /°C
- T. range 20 - 1000 °C
- Approx. Melting Point 1510 °C

Reference norms:
- ASTM B603 I 1.4765

ICRALLOY 20

Nominal Composition:
• Cr 19,0-22,0
• Al 4,5-5,0
• Si 1,0 max
• Mn 1,0 max
• C 0,10 max
• Fe rem.

Material Characteristics:

- Specific resist. at 20 °C 137 micro ohm/cm
- Density 7,20 g/cm3
- Temp. coefficient of resistance 70 km x 10-6 /°C
- T. range 20 - 1000 °C
- Approx. Melting Point 1510 °C

Reference norms:
- ASTM B603 IIB 1.4767